Abstract
A series of ferroelectric glass-ceramics was elaborated by the controlled growth of Ba(1-x)Sr(x)TiO(3) crystal particles in the glass system 60[Ba(1-y)Sr(y)]TiO(3)-10Al(2)O(3)-30SiO(2)(0≦y≦0.2) in molar basis. Analysis of crystal phases by X-ray diffraction revealed that Sr content in Ba(1-x)Sr(x)TiO(3) increased with increasing content of SrO in glasses by its preferential transfer into the crystal phase, and the appropriate temperature for the crystal growth was 1100°C. Curie temperatures of glass -ceramics shifted to lower temperature with increasing SrO content in the crystal and comparatively high dielectric constant was obtained at room temperature for a glass-ceramics with y=0.2. Frequency dependences of dielectric constant and loss tangent were examined in the frequency range from 1 K to 1 M Hz.
Published Date
1983-02-25
Publication Title
Memoirs of the School of Engineering, Okayama University
Publication Title Alternative
岡山大学工学部紀要
Volume
volume17
Issue
issue1
Publisher
岡山大学工学部
Publisher Alternative
School of Engineering, Okayama University
Start Page
97
End Page
105
ISSN